Products
Coating
Types and Features of Surface Insulation
Coating types -> | C-6A | C-9A | Remarks | |
Equivalent ASTM type | C-5 | C-5 | ||
Composition | organic/filler | organic/filler | ||
Thickness (um) | 0.40~0.60 | 1.00~1.20 | ||
Resistivity (Ωcm²/sheet)
|
Before SRA | ≥0.5 | ≥5.0 |
ASTM A717 SRA condition:750°C x 2hrs.In DX rich gas
|
After SRA | ≥0.1 | ≥0.5 | ||
Lamination factor (%) | 98 | 98 | 1.0 Mpat 0.05 in pressure (JIS C 2550) | |
Heat Resistance flaking after SRA
|
Not Recongnized | Not Recongnized | 150°C x 24hr in Air | |
Not Recongnized | Not Recongnized | 750°C x 2hrs.In DX rich gas | ||
Weathering (powdering) | Not Recongnized | Not Recongnized | 65°C, 95% humidity, 72hr | |
Adhesion (mmΦ)
|
Before SRA(mandrel bend tester) | 10 | 10 | ISO1519 |
After SRA(cross cut tester) | 5B | 5B | ASTM D3359B [0B(poor)~5B(excellent)] SRA | |
Resistance to Refrigerents
|
Change of surface | Not Recongnized | Not Recongnized |
R-134a/Freol @15C=65g/100g(1300C, 21day, 0.45μ.m filter paper)
|
Change of weight | Not Recongnized | Not Recongnized | ||
Weldability | excellent | good | Current : 100~150A, Ar99% flow.10~20L/min, Speed:0.25~0.50mpm |
Note: 1) Please designate surface insulation according to usage.Regarding coating properties,please contact us.
2) The coating thickness value and the resistivity is typical value, not guaranteed.